Hold the restoration by the IPS e.max CAD Crystallization Pin.

Spray the IPS e.max CAD Crystall./Glaze Spray directly on the unfired

IPS e.max CAD Crystall./Shades and Stains. Spray the restoration from all sides

while simultaneously rotating it.

Shake the spray can again between individual bursts.

Spray an even layer onto the restoration.

Allow the IPS e.max CAD Crystall./Glaze Spray to dry briefly until a whitish layer has formed.
If required, spray the restoration again to achieve an even Glaze Spray layer on the IPS e.max
CAD restoration.

Place the restoration in the center of the IPS e.max CAD Crystallization Tray and fire using the

stipulated parameters.

– If a maximum of 2 restorations to which the Glaze Spray has been applied are crystallized at the same time,

the Speed Crystallization/Glaze Spray can be used.

– If more than 2 restorations are crystallized, crystallization is carried out with the firing program

Crystallization/Glaze.